Hello. What exactly do we mean with methylated spirits? Pure methyl? pure ethanol? Mix methyl and ethanol? Something else? Thank you.
DANNYHOCKIN
DANNYHOCKIN
Supreme Being (105 reputation)Supreme Being (105 reputation)Supreme Being (105 reputation)Supreme Being (105 reputation)Supreme Being (105 reputation)Supreme Being (105 reputation)Supreme Being (105 reputation)Supreme Being (105 reputation)Supreme Being (105 reputation)
Group: Forum Members
Posts: 8, Visits: 79
Billis21 - 9/27/2017 11:14:36 PM
Hello. What exactly do we mean with methylated spirits? Pure methyl? pure ethanol? Mix methyl and ethanol? Something else? Thank you.

I believe it's the same as Denatured Alcohol. 
Can't wait to try this next week!

Fredrik Welen
Fredrik Welen
Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)
Group: Forum Members
Posts: 53, Visits: 478
Warren (Staff) - 8/26/2014 3:13:16 PM
Unfortunately the Zyvax infusion spray tack is no longer manufactured. 

In order to hold these individual pieces of carbon on the mould’s surface we need to use some sort of spray tack, however, all of the spray tacks (including all of the so called infusion tacks) leave visible marks when used on the surface of the mould. This is because they are all designed for gelcoated or painted parts and not clear finish parts that are generally the norm for carbon fibre work. To overcome this, we do the following:

Invisible Epoxy Infusion Spray-Tack

1.    Start with a clean, small plastic ‘spritser’ bottle (any openable plastic bottle with a pump-action mister spray, like for hair-care products).
2.    Mix up 10g of infusion resin with 3g of infusion hardener and pour into the bottle.
3.    Add 10g of metholated spirits to the bottle (it must be purple meths, no white spirit, acetone, alcohol or anything else).
4.    Shake the bottle thoroughly.
5.    Spray a thin film of the spray tack over the surface of the mould.
6.    Allow the meths to evaporate and wait around an hour or two for the epoxy to start reacting when it will become particularly tacky.
7.    Stick your reinforcement to the tacky mould surface.

When you do the infusion, you will find that the tiny amount of spray-tack on the surface will cross-link with the resin of the infusion epoxy and become completely invisible with not even a trace of anything on the surface of your parts!

I just tried this and used Easy lease as release agent.  It just crawl into small droplets and don´t smear out. Now I wounder how I will get it off. I just can´t seem to get a break in this project I am doing. Anyone knows were to get a invisable spray tack in EU europe suitable for resin infusion? 


Edited 4 Years Ago by Fredrik Welen
Lester Populaire
L
Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Fredrik Welen - 6/9/2022 5:05:25 PM
Warren (Staff) - 8/26/2014 3:13:16 PM
Unfortunately the Zyvax infusion spray tack is no longer manufactured. 

In order to hold these individual pieces of carbon on the mould’s surface we need to use some sort of spray tack, however, all of the spray tacks (including all of the so called infusion tacks) leave visible marks when used on the surface of the mould. This is because they are all designed for gelcoated or painted parts and not clear finish parts that are generally the norm for carbon fibre work. To overcome this, we do the following:

Invisible Epoxy Infusion Spray-Tack

1.    Start with a clean, small plastic ‘spritser’ bottle (any openable plastic bottle with a pump-action mister spray, like for hair-care products).
2.    Mix up 10g of infusion resin with 3g of infusion hardener and pour into the bottle.
3.    Add 10g of metholated spirits to the bottle (it must be purple meths, no white spirit, acetone, alcohol or anything else).
4.    Shake the bottle thoroughly.
5.    Spray a thin film of the spray tack over the surface of the mould.
6.    Allow the meths to evaporate and wait around an hour or two for the epoxy to start reacting when it will become particularly tacky.
7.    Stick your reinforcement to the tacky mould surface.

When you do the infusion, you will find that the tiny amount of spray-tack on the surface will cross-link with the resin of the infusion epoxy and become completely invisible with not even a trace of anything on the surface of your parts!

I just tried this and used Easy lease as release agent.  It just crawl into small droplets and don´t smear out. Now I wounder how I will get it off. I just can´t seem to get a break in this project I am doing. Anyone knows were to get a invisable spray tack in EU europe suitable for resin infusion? 


try spraying the spray tack onto the fabric.

Fredrik Welen
Fredrik Welen
Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)Supreme Being (767 reputation)
Group: Forum Members
Posts: 53, Visits: 478
I don´t know why i didn´t think of that. Thanks for reminding me.  I will add easy lease again and try again.
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Most infusion grade spray tacs are largely invisible. If they are causing you issues, you are probably using way too much. You don't need a lot - the vacuum should be doing most of the work. You just want to give a very very slight tac.

If you are really struggling, you can also try using an in-mould coating first, and then that will make your spray tac completely invisible regardless of how much you use.
chriscnf
c
Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)
Group: Forum Members
Posts: 34, Visits: 2.7K
Hanaldo - 6/26/2022 12:05:43 PM
Most infusion grade spray tacs are largely invisible. If they are causing you issues, you are probably using way too much. You don't need a lot - the vacuum should be doing most of the work. You just want to give a very very slight tac.

If you are really struggling, you can also try using an in-mould coating first, and then that will make your spray tac completely invisible regardless of how much you use.

Which spray are you using now Hanaldo?
Lester Populaire
L
Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
chriscnf - 6/27/2022 7:38:38 AM
Hanaldo - 6/26/2022 12:05:43 PM
Most infusion grade spray tacs are largely invisible. If they are causing you issues, you are probably using way too much. You don't need a lot - the vacuum should be doing most of the work. You just want to give a very very slight tac.

If you are really struggling, you can also try using an in-mould coating first, and then that will make your spray tac completely invisible regardless of how much you use.

Which spray are you using now Hanaldo?

For visual applications i like to use isotacker from sicomin, and aerofix 2 for everything else as this one is much tackier and easier to work with. Used some other stuff when visiting other workshops and can't say there is a night and day difference between all the products I worked with.
The isotacker does completely dissolve which is nice when used on the tool directly tho.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search