	Group: AdministratorsPosts: 2.5K, 
    Visits: 8.5K
 
 | 
                    
			            Remember that EasyLease is hydroscopic so if you have had the lid left off or not fully sealed and/or you open it a lot, that will degrade it quicker.  Also if your moulds post cure was not done properly, that may cause issues too.                 
			            
 Warren Penalver