Hello,

Since a while all my new moulds keep failing on releasing the carbon.
All moulds are cured and polished and use a minimum of 5 chemical release layers.

All is made in the autoclave but never had these problems with other moulds made from the same material.

Even now the mould sticks on the carbon and cant even get it loose with a hammer.
Can the chemical release agent get too old to work? do i need to shake it?









Edited 5 Years Ago by Thomb
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search