how can i avoid the gelcoat puddling up when brushing it on.   i used 7 layers of easy leaze and 2 coats of mirror glaze 88 wax  but it ends up puddling together as water in a bucket of oil.

help please.
Reply
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Just for info, East Coast Fibreglass do the brush-applicable version of this if you'd like to avoid needing to use an additive in future. If you look under 'Specialist gelcoats' you should find it. As far as I'm aware, it's the same product but formulated for brush application, rather than spray. 