By jeffrey bres - 9/20/2020 10:32:39 AM
how can i avoid the gelcoat puddling up when brushing it on. i used 7 layers of easy leaze and 2 coats of mirror glaze 88 wax but it ends up puddling together as water in a bucket of oil.
help please.
|
By jeffrey bres - 3/1/2021 12:01:08 PM
I dont. At my first try i used 1 theespoon. Now 1.5 theespoon for each 100ml of gelcoat. .i dont realy see it coulding up.. i mix 24h before i apply at least. But in my case i dont need 100% transparent. Its no isseu if i have some cloudy finish. But yes i agree 100% overdo it and it will be white ish..
|
|