Group: Forum Members
Posts: 1,
Visits: 1
|
hi, i did my first river table and left to dry for a week. its 30 mm deep, i did it in 3 pours. top seemed dry and hard but when i flippy the work over to remove the plastic sheet i had laid it on its very sticky, obviously a bad mix or temperature issue, any ideas how to get the sticky mess off. its a nightmare, please help
|