Here is a picture of a plug with gel coat on it.  What would be your recomendations for infusing this. Keep in mind once this is a mold it will be basically a U-shaped mold. The kick out you can see in the picture is not on the other side. the other side is smooth.  The lowered sections in front and back (left to right) are flange area. The part area is 32" (813mm)long. The max height is 16"(406mm) and the max width is 16"(406mm).

 I really only see two options....

1. Infuse from the side and let the resin go out along the flange in the spiral then go down one side of the U and back up the other side of the U....

2. Infuse from the end and have the resin as it enters have to climb up the walls of the U in the spiral then across the part.....

Any sugestions would be greatly appreciated. Please be specific as to where I should run the spiral.

Thanks,   Dennis
Attachments
Tranny-tunnel-gel.jpg (853 views, 909.00 KB)
Edited 14 Years Ago by Dennis G
Reply
Warren
Warren
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Administrators
Posts: 214, Visits: 783
cool idea!!

I presume the car this is going in is spaceframed or has adequate structural support to cut out the tunnel and replace with carbon??

Great weight saving over steel.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dennis G - 14 Years Ago
wozza - 14 Years Ago
     2 part mould
Jack.Strong - 14 Years Ago
Matt (Staff) - 14 Years Ago
Dennis G - 14 Years Ago
wozza - 14 Years Ago
_GABBER - 14 Years Ago
Dennis G - 14 Years Ago
wozza - 14 Years Ago
Warren - 14 Years Ago
_GABBER - 14 Years Ago
Dennis G - 13 Years Ago
Dennis G - 13 Years Ago
Ashfaq - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search