	Group: Awaiting Activation 	        
    Posts: 1, 
    Visits: 4 
    
 
          
		     | 
				                       
                 
                
                    
			            I want to use RI for a project but am abit confused about the resin to use
  When the molds were delivered they came with this note:
  Molds: Each of the molds used for manufacture will be constructed using a CCP gel coat layer of 20-40 mills backed up with a surface veil and 3-10mm of hand laid chop mat and Hydrex vinyl ester resin. This will be backed up with 10-20mm of Optiplex tooling resin and chopped glass.
  All tools will be mounted to backup structure with foam and fiberglass standoffs to eliminate and any future print through or mark off in the plug surface from the back up structure.
  Molds will be suitable for heated vacuum bag or clamping pressure molding up to 5 tons of pressure and 250 deg f. 
  So which resin would you use vinylester?
  The job is for an underwater glider about 1m x 1m easy curves