fgayford (21/12/2012)


Hi Dean

As far as I know you pretty much must use epoxy resin for  infusion if using carbon fiber to get the best mechanical strength.

It doesn't really matter what the mold is made of as long as you have a good release system in place..

Fred


I've heard that if youre infusing with epoxy and the mould is polyester based, you need to posture the mould to bake the styrene out of it, otherwise you'll get release problems. I need clarification on this.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
You can get low viscosity polyester resin to use for infusion but this obviously has the normal downfalls and has to be infused at -0.8 bar at most
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
dean legg (05/12/2012)
I want to use RI for a project but am abit confused about the resin to use

When the molds were delivered they came with this note:

Molds: Each of the molds used for manufacture will be constructed using a CCP gel coat layer of 20-40 mills backed up with a surface veil and 3-10mm of hand laid chop mat and Hydrex vinyl ester resin. This will be backed up with 10-20mm of Optiplex tooling resin and chopped glass.

All tools will be mounted to backup structure with foam and fiberglass standoffs to eliminate and any future print through or mark off in the plug surface from the back up structure.

Molds will be suitable for heated vacuum bag or clamping pressure molding up to 5 tons of pressure and 250 deg f.

So which resin would you use vinylester?

The job is for an underwater glider about 1m x 1m easy curves

 

Thanks Dean


Hi Dean

As far as I know you pretty much must use epoxy resin for  infusion if using carbon fiber to get the best mechanical strength.

It doesn't really matter what the mold is made of as long as you have a good release system in place..

Fred
dean legg
dean legg
Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)
Group: Awaiting Activation
Posts: 1, Visits: 4
I want to use RI for a project but am abit confused about the resin to use

When the molds were delivered they came with this note:

Molds: Each of the molds used for manufacture will be constructed using a CCP gel coat layer of 20-40 mills backed up with a surface veil and 3-10mm of hand laid chop mat and Hydrex vinyl ester resin. This will be backed up with 10-20mm of Optiplex tooling resin and chopped glass.

All tools will be mounted to backup structure with foam and fiberglass standoffs to eliminate and any future print through or mark off in the plug surface from the back up structure.

Molds will be suitable for heated vacuum bag or clamping pressure molding up to 5 tons of pressure and 250 deg f.

So which resin would you use vinylester?

The job is for an underwater glider about 1m x 1m easy curves

Thanks Dean
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search