fgayford (21/12/2012)
Hi Dean
As far as I know you pretty much must use epoxy resin for  infusion if using carbon fiber to get the best mechanical strength.
It doesn't really matter what the mold is made of as long as you have a good release system in place..
Fred
I've heard that if youre infusing with epoxy and the mould is polyester based, you need to posture the mould to bake the styrene out of it, otherwise you'll get release problems. I need clarification on this.