Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Yes that is correct, a single layer top up is usually all that is needed. If you need to more aggressively clean the mould using mould cleaner or anything more aggressive than a damp cloth, then you risk stripping off the release agent so we would recommend fully cleaning to remove all traces and starting afresh to be on the safe side.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|