By carbon man - 7/6/2020 6:18:05 PM
I have had a successful pull from first mould where I applied 7 coats of easy lease. The next time I use this mould is 1 layer of easy lease enough?
|
By Warren (Staff) - 7/10/2020 9:35:20 AM
Yes that is correct, a single layer top up is usually all that is needed. If you need to more aggressively clean the mould using mould cleaner or anything more aggressive than a damp cloth, then you risk stripping off the release agent so we would recommend fully cleaning to remove all traces and starting afresh to be on the safe side.
|
|