Hi guys!

Have been following you for many years and always been inspired by your YouTube tutorials!

I have a front splitter for my track car that I purchased not long ago and they don’t make it anymore so I’m wanting to make a mould of it incase it gets damaged but more to the fact I would like to make it out of carbon fibre.

It has many angles which means it can’t be made from a single piece mould, I was thinking a 2 piece split or even 3? consisting of a top and bottom so to speak

I would very much like your opinion and any advice you could give me in this venture, the splitter is in 2 parts and pictured is one one half as the other half is a mirror image.... also the aluminium plate bonded to the bottom will be removed For mould making

I have uploaded the pictures to my one drive via a link as o tried to upload the pictures straight to here but after 15mins of waiting it still hadn’t uploaded one picture.

https://1drv.ms/u/s!ApxzGlwLzg9QhTgOgj0AJpMaPCjM?e=sardGQ

Hope you can assist me
Thanks
Phil
Reply
beliblisk
b
Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)
Group: Forum Members
Posts: 53, Visits: 2.8K
Infusion shouldnt be a problem. Little spray tack and this can be done without any major weave distortions (its quite easy for places where fingers fit).

If its really tricky gometry perhaps home made prepreg is the way to goSmile 
Edited 5 Years Ago by beliblisk
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
export001 - 5 Years Ago
Hanaldo - 5 Years Ago
export001 - 5 Years Ago
Steve Broad - 5 Years Ago
export001 - 5 Years Ago
beliblisk - 5 Years Ago
Hanaldo - 5 Years Ago
export001 - 5 Years Ago
Hanaldo - 5 Years Ago
export001 - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search