		| By export001 - 6/4/2020 8:01:07 PM 
 Hi guys!
 
 Have been following you for many years and always been inspired by your YouTube tutorials!
 
 I have a front splitter for my track car that I purchased not long ago and they don’t make it anymore so I’m wanting to make a mould of it incase it gets damaged but more to the fact I would like to make it out of carbon fibre.
 
 It has many angles which means it can’t be made from a single piece mould, I was thinking a 2 piece split or even 3? consisting of a top and bottom so to speak
 
 I would very much like your opinion and any advice you could give me in this venture, the splitter is in 2 parts and pictured is one one half as the other half is a mirror image.... also the aluminium plate bonded to the bottom will be removed For mould making
 
 I have uploaded the pictures to my one drive via a link as o tried to upload the pictures straight to here but after 15mins of waiting it still hadn’t uploaded one picture.
 
 https://1drv.ms/u/s!ApxzGlwLzg9QhTgOgj0AJpMaPCjM?e=sardGQ
 
 Hope you can assist me
 Thanks
 Phil
 |  
		| By export001 - 6/7/2020 7:55:40 AM 
 Will keep that in mind! I’m making a few other moulds of smaller easier items before I take this on, but all advice is appreciated for when I do this part 😁
 |  |