Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Should be fine, it's not really a functional splitter it's really just a cosmetic lip. So it doesn't need to be super strong. Put a couple of extra layers around the mounting points and that will be plenty.
For the flow mesh, don't bother trying to go around the leading edge, just butt up into it from the top and bottom. The resin will flow an inch or two with no mesh, and that radius will be your biggest challenge with bridging and removing the consumables afterwards.
|