Has anyone converted a tyre compressor and made it into a vacuum pump to draw resin into a mould... would it be powerful enough?
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
No, venturies can't pull a full vacuum, they only reach about 27in/hg. Infusion needs very high vacuum to give good results, atleast 29.9in/hg. 