Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Tyre Compressor Conversion For Vacuum
Tyre Compressor Conversion For Vacuum
Post Reply
Like
8
Tyre Compressor Conversion For Vacuum
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
dilligaf76
dilligaf76
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 115
Has anyone converted a tyre compressor and made it into a vacuum pump to draw resin into a mould... would it be powerful enough?
Reply
Like
8
Hanaldo
Hanaldo
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
No, venturies can't pull a full vacuum, they only reach about 27in/hg. Infusion needs very high vacuum to give good results, atleast 29.9in/hg.
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search