Hi, I am trying to cast Smooth On Crystal Clear 202 inside a pressure pot at 55 psi. The surface is very spiky. First I thought it might be moisture in the air coming from the compressor but it’s still does it even after fitting a moisture trap. Any insight to what the problem might be?
Reply
Jcmarti
J
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 2, Visits: 7
I'm doing a vacuum infusion glass lay up. The problem I'm have is my product is coming out with orange peel finish instead of glossy. Using a Partall PVA #10 mold release. 