Hi, I am trying to cast Smooth On Crystal Clear 202 inside a pressure pot at 55 psi. The surface is very spiky. First I thought it might be moisture in the air coming from the compressor but it’s still does it even after fitting a moisture trap. Any insight to what the problem might be?
|