You may be demoulding too soon and getting a bit of print through.
PVA is not the best for surface finish. Often if leaves a bit of surface marring that needs a light sand and polish to remove, so that may be part of the problem.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|