JUST SO YOU KNOW


Author
Message
Daz
Daz
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 93, Visits: 651
I have used some cheap spray glue to hold my carbon reinforcement in the mold whilst laminating up

Not alot just a quick squirt

Yes its gone off and hard but you can peel the laminate apart

so be warned,!!!!  

I will be getting the real stuff when available :-)
Reply
Kevin-Lee
Kevin-Lee
Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)
Group: Forum Members
Posts: 44, Visits: 2.4K
Hi Daz,

I have also noticed this. It almost seems like the carbon is not even fully wetting out, the resin is just between the nodes and not between the individual filaments and it all just becomes one big expensive peel ply...

Kev.