By Daz - 11/27/2012 7:26:57 PM				
            
                      
            I have used some cheap spray glue to hold my carbon reinforcement in the mold whilst laminating up
  Not alot just a quick squirt
  Yes its gone off and hard but you can peel the laminate apart
  so be warned,!!!!  
  I will be getting the real stuff when available :-)
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By mikew - 12/4/2012 4:25:42 PM				
            
                      
            I've been using a product called Elmers repositionable spray.  I just give a gentle spray on the fabric, not the mould, wait 5 minutes then position it. No issues with delaminating.
           
		 | 			
		 
	
	
						
		 	
		
	 |