I have used some cheap spray glue to hold my carbon reinforcement in the mold whilst laminating up

Not alot just a quick squirt

Yes its gone off and hard but you can peel the laminate apart

so be warned,!!!!  

I will be getting the real stuff when available :-)
Reply
mikew
mikew
Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)
Group: Forum Members
Posts: 56, Visits: 128
I've been using a product called Elmers repositionable spray.  I just give a gentle spray on the fabric, not the mould, wait 5 minutes then position it. No issues with delaminating.