I'm before making my rear engine lid. As the lid got place for rear number plate I was thinking if I could insert wireing underneath the CF bonnet. 
I know normally heating in aerospace is installed inside the composite part and on the ends are plugs.
Is it possible just to use normal wires? But then it will have to come out through the bag to not being soaked with resin.
Distance I'm thinking of is with red line.


Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I wouldn't, you're making life very difficult for yourself, especially for infusion. Why do you want to do it?
Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
Hanaldo - 2/1/2020 10:00:45 AM
I wouldn't, you're making life very difficult for yourself, especially for infusion. Why do you want to do it?

I building aerospace.seals for living.Build next door which is part of same company they do air intakes for helicopters which are heated.So I thought the wireing could be done for electrics.Different is they do prepreg and I doing infiusion.I could have cables integrated in the part.