Group: Forum Members
Posts: 311,
Visits: 13K
|
I built race car parts with integrated electronics and cables in infusion and prepreg. It is certainly possible, but for your application i cannot see the advantage. I would rather integrate a cable channel so you have a neat solution to hide the cables, but everything remains independent so you can switch things out.
|