Resin infusion of a carbon fibre honeycomb sandwivh structure


Author
Message
Hadi Koshairy
Hadi Koshairy
Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)
Group: Forum Members
Posts: 4, Visits: 9
Hello,
I want to make a complex structure composed of a carbon fiber, Aluminum honeycomb sandwich structure resin infusion. My problem is that while applying resin infusion I want to ensure that the carbon fiber sticks the aluminum honeycomb and at the same time ensure that the amount of epoxy entering the honeycomb is minimum. Can someone please help. Note: putting the honeycomb above the carbon fiber is not an option in my case.
Best regards,
Hadi ElKoshairy
Replies
Hanaldo
Hanaldo
Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh you simply can't use honeycomb in an infusion process, it has to be bonded on after the infused skin(s) have cured.
Hadi Koshairy
Hadi Koshairy
Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)
Group: Forum Members
Posts: 4, Visits: 9
Hanaldo - 10/18/2019 9:04:56 PM
Yeh you simply can't use honeycomb in an infusion process, it has to be bonded on after the infused skin(s) have cured.

Is there a way where you can put a layer over the honeycomb to ensure that no resin will enter during the infusion process??