			            You make the moulds in one shot. Make one half, let it cure, release agent the flange, make the other.  They will line up perfectly then.  You can even make registration dots on the flange so it aligns perfectly every time.  Then you can bolt the 2 halves together when the time comes.                 
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |