Hi guys, based on your experiences for years in vacuum infusion, what type of release agents do you recommend?
There are waxes, liquid waxes, pva, semi-permanent.. what type of product and brand have you been successful with?
We are open to talk about other products here that are not available in easycomposites? there are a lot of brands.

Regards.

Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Definitely semi-perms, there's just no competition. Different generation of release system. Like comparing an iPhone to a Nokia 3315.