By Geteda - 6/6/2019 1:38:37 AM
Hi guys, based on your experiences for years in vacuum infusion, what type of release agents do you recommend? There are waxes, liquid waxes, pva, semi-permanent.. what type of product and brand have you been successful with? We are open to talk about other products here that are not available in easycomposites? there are a lot of brands.
Regards.
|
By Geteda - 6/7/2019 2:28:01 AM
Thank you for sharing your experiences, I want to try these techniques with semi-permanent and waxes, also waxes with pva in infusions.
I have a question, is there a way to reduce the viscosity of the pva to use it with cloths as with waxes?
|
|