Hi guys, based on your experiences for years in vacuum infusion, what type of release agents do you recommend?
There are waxes, liquid waxes, pva, semi-permanent.. what type of product and brand have you been successful with?
We are open to talk about other products here that are not available in easycomposites? there are a lot of brands.

Regards.

Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Feel free to talk about other brands here.

We recommend semi-permanents for infusion due to the reliability and ease of release. If you have watched our bonnet making video, you will see the bonnet top layer pretty much fall out the mould with no effort - that is due to good application of a semi-permanent release agent.  Our version we rate highly and can be found here: Easy-Lease Chemical Release Agent

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search