High temperatures resins


Author
Message
Slamhammer
S
Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)
Group: Forum Members
Posts: 4, Visits: 7
I am looking for information on what resin to use in a high temperature project. It needs to be good up to 400 celcius.
Reply
Slamhammer
S
Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)
Group: Forum Members
Posts: 4, Visits: 7
Hanaldo - 4/7/2019 2:05:45 PM
Kind of out of thermoset resin territory, especially for resin infusion. I doubt there's any commercially available pre-pregs that could get up there either, that's getting close to needing ceramic.

Going to be a handgaurd for a rifle. It won't touch the barrle, but it will get close.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search