+x scottracing - 4/7/2019 8:30:15 PMlots of thermosets can be postcured up to 200degrees, where are you located? It would be best speaking to your local reseller and seeing what they stock.
+x scottracing - 4/7/2019 7:22:20 PMi dont think you will need something that goes to that high temp if its a handguard, you can use insulator materials between the barrel and thecomposite part to allow for that. Theres plenty of coatings around even self adhesive alu tape will work.
+x Hanaldo - 4/7/2019 2:05:45 PMKind of out of thermoset resin territory, especially for resin infusion. I doubt there's any commercially available pre-pregs that could get up there either, that's getting close to needing ceramic.