I have seen more than one video that indicates they have used both a peel ply and a perforated release ply. on the same laminated item.
In one video they demonstrated the difference between these two products and how the release ply was easier to remove than the peel ply but they did this for demonstration purposes only.
What would be the need for using both materials together?


A Lifelong Learner

Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
HansenJC - 2/18/2019 4:49:09 AM
I have seen more than one video that indicates they have used both a peel ply and a perforated release ply. on the same laminated item.
In one video they demonstrated the difference between these two products and how the release ply was easier to remove than the peel ply but they did this for demonstration purposes only.
What would be the need for using both materials together?

I use strips of perforated film under flow channels like the enka channel (on top of peel ply) so that the cured resin filled channels  are much easier to remove from the finished parts.





Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Just makes it easier to remove the infusion mesh, but still keeps the peel ply finish.
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As Hanaldo says - especially on complex shapes.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search