By HansenJC - 2/18/2019 4:49:09 AM

I have seen more than one video that indicates they have used both a peel ply and a perforated release ply. on the same laminated item.
In one video they demonstrated the difference between these two products and how the release ply was easier to remove than the peel ply but they did this for demonstration purposes only.
What would be the need for using both materials together?
By Warren (Staff) - 2/18/2019 1:07:02 PM

As Hanaldo says - especially on complex shapes.