I have seen more than one video that indicates they have used both a peel ply and a perforated release ply. on the same laminated item.
In one video they demonstrated the difference between these two products and how the release ply was easier to remove than the peel ply but they did this for demonstration purposes only.
What would be the need for using both materials together?


A Lifelong Learner

Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As Hanaldo says - especially on complex shapes.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search