I present this pict for beloved Talkcomposites forum member, may can help your lastest project.

 

Process:

Resin Infusion

Composition:

1 layer of Carbon fibre 2/2twill 200gr

2 layer of Fibre glass WR 290gr

300gr oof epoxy resin

Finishing:

Spies hacker plastic primer 3 coat

Spies hacker clear coat 4 coat






















Edited 13 Years Ago by Leon
Replies
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
looks great, thanks for sharing those pictures!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Leon
Leon
Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)
Group: Forum Members
Posts: 59, Visits: 606
matthieutje65 (27/10/2012)
looks great, thanks for sharing those pictures!


your welcome matthieu..Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Leon - 13 Years Ago
prairiecustomcomposites - 13 Years Ago
Leon - 13 Years Ago
matthieutje65 - 13 Years Ago
Leon - 13 Years Ago
NikCFC - 13 Years Ago
Leon - 13 Years Ago
WilliamsHPF - 13 Years Ago
NikCFC - 13 Years Ago
Leon - 13 Years Ago
NikCFC - 13 Years Ago
Leon - 13 Years Ago
brasco - 12 Years Ago
Extreme - 12 Years Ago
carbonlynx - 12 Years Ago
     Very very nice!
Demlotcrew - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search