Hii,

I present this pict for beloved Talkcomposites forum member, may can help your lastest project.

 

Process:

Resin Infusion

Composition:

1 layer of Carbon fibre 2/2twill 200gr

2 layer of Fibre glass WR 290gr

300gr oof epoxy resin

Finishing:

Spies hacker plastic primer 3 coat

Spies hacker clear coat 4 coat






















Edited 13 Years Ago by Leon
Reply
Leon
Leon
Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)
Group: Forum Members
Posts: 59, Visits: 606
Here we go, the Nissan skyline GTR  engine cover. 
This part is extremely tricky to work with resin infusion, the most critical steps is set up the CF on the mould without any spotlight distortion weave, there are some trick I would like to share. As you can see below that the part has already one, but i decide to mould it again because I got a orange peel conture on the mould and also the part may you can't  spot it at pict. Yes, first I spray poxy filler for 3 times then wet sanded to remove the peel orange surface. The pict how to set up the CF part will be post here soon after I finish the mould.




It's made from carbon fibre/4 layer because of  high temp replacement part.

Regards

Leon
Edited 13 Years Ago by Leon
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Leon - 13 Years Ago
prairiecustomcomposites - 13 Years Ago
Leon - 13 Years Ago
matthieutje65 - 13 Years Ago
Leon - 13 Years Ago
NikCFC - 13 Years Ago
Leon - 13 Years Ago
WilliamsHPF - 13 Years Ago
NikCFC - 13 Years Ago
Leon - 13 Years Ago
NikCFC - 13 Years Ago
Leon - 13 Years Ago
brasco - 12 Years Ago
Extreme - 12 Years Ago
carbonlynx - 12 Years Ago
     Very very nice!
Demlotcrew - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search