By Leon - 10/27/2012 4:16:29 PM
Hii,
I present this pict for beloved Talkcomposites forum member, may can help your lastest project.
Process:
Resin Infusion
Composition:
1 layer of Carbon fibre 2/2twill 200gr
2 layer of Fibre glass WR 290gr
300gr oof epoxy resin
Finishing:
Spies hacker plastic primer 3 coat
Spies hacker clear coat 4 coat










|
By Demlotcrew - 5/23/2013 12:30:54 PM
Very very nice!
|
|