Dear Sir, yesterday I have received my order, gelcoat GC50, and found that it is very jelly or thick. I need to apply it by spraying to obtain a relatively thin and uniform layer. I have a spray gun with 2mm nozzle.
My feeling is that I need to dilute the gelcoat with styrene monomer. Please can you suggest how to do it without loosing gelcoat proprieties? What weight percentage of styrene can be added? 
Many thanks in advance, best regards,
Miroslav
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The formulation changed around 5 years ago.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Miroslav - 8 Years Ago
Warren (Staff) - 8 Years Ago
MarkMK - 8 Years Ago
Warren (Staff) - 8 Years Ago
Nishitate Luis - 8 Years Ago
Warren (Staff) - 8 Years Ago
Nishitate Luis - 8 Years Ago
MarkMK - 8 Years Ago
Warren (Staff) - 8 Years Ago
Hanaldo - 8 Years Ago
Nishitate Luis - 8 Years Ago
SHaas - 8 Years Ago
Warren (Staff) - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search