Dear Sir, yesterday I have received my order, gelcoat GC50, and found that it is very jelly or thick. I need to apply it by spraying to obtain a relatively thin and uniform layer. I have a spray gun with 2mm nozzle.
My feeling is that I need to dilute the gelcoat with styrene monomer. Please can you suggest how to do it without loosing gelcoat proprieties? What weight percentage of styrene can be added? 
Many thanks in advance, best regards,
Miroslav
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The formulation of GC50 has changed slightly since the video was published (there is a pop up box).  The new formulation does not become tacky with acetone so that technique does not work with the current version of GC50.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Nishitate Luis
N
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 4, Visits: 25
Thanks for your answer, what technique can I use now to stick the carbon fiber? I do infusion and needed to stick well to the mold so that I do not have bubbles.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Miroslav - 7 Years Ago
Warren (Staff) - 7 Years Ago
MarkMK - 7 Years Ago
Warren (Staff) - 7 Years Ago
Nishitate Luis - 7 Years Ago
Warren (Staff) - 7 Years Ago
Nishitate Luis - 7 Years Ago
MarkMK - 7 Years Ago
Warren (Staff) - 7 Years Ago
Hanaldo - 7 Years Ago
Nishitate Luis - 7 Years Ago
SHaas - 7 Years Ago
Warren (Staff) - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search