Group: Forum Members
Posts: 4,
Visits: 25
|
hello, I just tried the gelcoat GC50, a test with air gun and another with a brush, and my problem is when I put the carbon fiber, I try to stick it to the mold with acetone as in the tutorial but the carbon fiber does not stick, What I can be doing wrong?
|