Dear Sir, yesterday I have received my order, gelcoat GC50, and found that it is very jelly or thick. I need to apply it by spraying to obtain a relatively thin and uniform layer. I have a spray gun with 2mm nozzle.
My feeling is that I need to dilute the gelcoat with styrene monomer. Please can you suggest how to do it without loosing gelcoat proprieties? What weight percentage of styrene can be added? 
Many thanks in advance, best regards,
Miroslav
Reply
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Adding to Warren's advice, you'll find that you'll get better results using a bigger nozzle also

If using the recommended G100 cup gun set-up, the FN6 (4.7mm) or, perhaps, the next size down will give good results. It will likely spray okay, if warm, through a 2mm nozzle but it will take a long time to achieve good coverage on anything but quite small moulds



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Miroslav - 7 Years Ago
Warren (Staff) - 7 Years Ago
MarkMK - 7 Years Ago
Warren (Staff) - 7 Years Ago
Nishitate Luis - 7 Years Ago
Warren (Staff) - 7 Years Ago
Nishitate Luis - 7 Years Ago
MarkMK - 7 Years Ago
Warren (Staff) - 7 Years Ago
Hanaldo - 7 Years Ago
Nishitate Luis - 7 Years Ago
SHaas - 7 Years Ago
Warren (Staff) - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search