Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
1200 is wayyyy too fine for a pattern coating like high gloss coat. Need about 240 at the finest, preferably 180.
In any case, unless the plug came out of the mould and only left the gloss coat on the surface, then that isn't your issue - just thought I'd mention it.
|