We are casting a complex part with a lot of sharp and opposing angles, which has proven to be extremely difficult to accomplish with a single sheet layup. While we did close in on the goal, the method proved to be unsound. Changing methods, the best results have come from approaching the layup with multiple carbon fiber pieces. This required a lot of precise cuts and matching of weave, as you might imagine. The problem now is that we get stray, quite noticeable, carbon fiber 'fragments' in our parts. My question is to know if there is a way to apply some type of temporary backing to a section of non-prepreg roll which would keep the weave intact to allow me to cut and lay out the shapes I need and reduce stray fragments, then being able to peel off the backing upon layup.
There is one YouTube video of an Aussie showing how to apply a mix of PVA/H2O and thin 'paper' which dried as a backing which you can then peel off in layup. That didn't work for us. Is prepreg the only answer? I would also think that since we're spraying clear gel coat in the mold before layup, any PVA would ruin the bond between the resin and gel coat. Is there a resin soluble product that we could bond the carbon fiber and paper with? We also use spray adhesive to keep a couple of key parts in place which claims to dissolve in resin but that seems to risky.

The templates in the picture attached are a few of the shapes that we need perfect.
Thanks for any help,
Sr. Nerd Lab Technician 

Edited 8 Years Ago by Nerd Lab
drippy
drippy
Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)
Group: Forum Members
Posts: 32, Visits: 388
I have never used this product before but looks really interesting and seems to keep the carbon together not too bad. The link talks more about it.  https://compositeenvisions.com/carbon-fiber-fabric-2x2-twill-3k-203-43gsm-6oz-50-toray-t-300-with-web-lock-stabilization-1960.html . I have also seen carbon that has scrim on the back that helps keep the fibers together. 

Edited 8 Years Ago by drippy
oekmont
oekmont
Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Or you could use spray adhesive to bond the second layer on the backside of the first. This stops fraying and keeps the cloth more flexible compared to the fixed commercial cloths.

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Exactly what oekmont said.
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
A stabilised fabric like the one above or our version ProFinish Carbon Fibre will do the job fine, or as okemont suggested. People have even used hairsprays and all sorts of things in the past but probably best stick to stuff that is unlikely to cause any other issues.



Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Nerd Lab
Nerd Lab
Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)
Group: Forum Members
Posts: 6, Visits: 42
drippy - 8/3/2018 5:14:30 AM
I have never used this product before but looks really interesting and seems to keep the carbon together not too bad. The link talks more about it.  https://compositeenvisions.com/carbon-fiber-fabric-2x2-twill-3k-203-43gsm-6oz-50-toray-t-300-with-web-lock-stabilization-1960.html . I have also seen carbon that has scrim on the back that helps keep the fibers together. 

I'll look into this, thank you. Do you remember where you saw / what company had this product with scrim on the back?

Nerd Lab
Nerd Lab
Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)
Group: Forum Members
Posts: 6, Visits: 42
oekmont - 8/3/2018 6:17:20 AM
Or you could use spray adhesive to bond the second layer on the backside of the first. This stops fraying and keeps the cloth more flexible compared to the fixed commercial cloths.

Definitely worth a shot. Do you have any recommendations for a flexible cloth that would be use in this application? Thank you for the suggestion.

Nerd Lab
Nerd Lab
Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)
Group: Forum Members
Posts: 6, Visits: 42
Warren (Staff) - 8/3/2018 8:23:03 AM
A stabilised fabric like the one above or our version ProFinish Carbon Fibre will do the job fine, or as okemont suggested. People have even used hairsprays and all sorts of things in the past but probably best stick to stuff that is unlikely to cause any other issues.


I agree. Let's not add more variables. Thank you for the response and for the link.

Nerd Lab
Nerd Lab
Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)Supreme Being (76 reputation)
Group: Forum Members
Posts: 6, Visits: 42
drippy - 8/3/2018 5:14:30 AM
I have never used this product before but looks really interesting and seems to keep the carbon together not too bad. The link talks more about it.  https://compositeenvisions.com/carbon-fiber-fabric-2x2-twill-3k-203-43gsm-6oz-50-toray-t-300-with-web-lock-stabilization-1960.html . I have also seen carbon that has scrim on the back that helps keep the fibers together. 

Thank you for this. Do you remember where you might have seen the carbon fiber with scrim backing? 

drippy
drippy
Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)Supreme Being (471 reputation)
Group: Forum Members
Posts: 32, Visits: 388
Nerd Lab - 8/3/2018 2:15:57 PM

Thank you for this. Do you remember where you might have seen the carbon fiber with scrim backing? 

I'm trying to look online for the place that sells it. I have seen it used in videos of people making parts. Take a look at this post from another forum. This guy is explaining how he adds veneer to the back of the carbon his is cutting and he has pics to help.  https://www.ducati.ms/forums/241-tech-forum/628658-how-cut-non-fraying-edge-carbon-fiber.html .. Hopefully this can help a little too. 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search