+x drippy - 8/3/2018 5:14:30 AMI have never used this product before but looks really interesting and seems to keep the carbon together not too bad. The link talks more about it. https://compositeenvisions.com/carbon-fiber-fabric-2x2-twill-3k-203-43gsm-6oz-50-toray-t-300-with-web-lock-stabilization-1960.html . I have also seen carbon that has scrim on the back that helps keep the fibers together.
+x oekmont - 8/3/2018 6:17:20 AMOr you could use spray adhesive to bond the second layer on the backside of the first. This stops fraying and keeps the cloth more flexible compared to the fixed commercial cloths.
+x Warren (Staff) - 8/3/2018 8:23:03 AMA stabilised fabric like the one above or our version ProFinish Carbon Fibre will do the job fine, or as okemont suggested. People have even used hairsprays and all sorts of things in the past but probably best stick to stuff that is unlikely to cause any other issues.
+x Nerd Lab - 8/3/2018 2:15:57 PMThank you for this. Do you remember where you might have seen the carbon fiber with scrim backing?