The new degassing system


Author
Message
BananeDC
B
Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)
Group: Forum Members
Posts: 15, Visits: 14
Thanks Warren. Is it ok with white gas ?

Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As far as I can tell, white gas is pure petrol.  Petrol is not recommended for use on acrylic based plastics as it may dull the surface.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
BananeDC
B
Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)
Group: Forum Members
Posts: 15, Visits: 14
ok thanks !

BananeDC
B
Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)
Group: Forum Members
Posts: 15, Visits: 14
Can i find it in supermarkets ?

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Isopropyl alcohol is commonly sold as a surface cleaner for applying automotive vinyl wraps. You might find it in a supermarket if it has a small car care section. Otherwise check your local automotive stores or a chemist or hardware. It is common stuff, should be easy to find.
BananeDC
B
Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)Supreme Being (120 reputation)
Group: Forum Members
Posts: 15, Visits: 14
Thanks Hanaldo !

Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hanaldo - 7/12/2018 11:10:29 PM
Isopropyl alcohol is commonly sold as a surface cleaner for applying automotive vinyl wraps. You might find it in a supermarket if it has a small car care section. Otherwise check your local automotive stores or a chemist or hardware. It is common stuff, should be easy to find.

Most 'screen wipes' for computer screens or tattoo wipes (for wiping the skin before or after a tattoo) also use IPA.


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search