Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hanaldo - 7/12/2018 11:10:29 PM
Isopropyl alcohol is commonly sold as a surface cleaner for applying automotive vinyl wraps. You might find it in a supermarket if it has a small car care section. Otherwise check your local automotive stores or a chemist or hardware. It is common stuff, should be easy to find.

Most 'screen wipes' for computer screens or tattoo wipes (for wiping the skin before or after a tattoo) also use IPA.


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
BananeDC
B
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 15, Visits: 14
Thanks Hanaldo !

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Isopropyl alcohol is commonly sold as a surface cleaner for applying automotive vinyl wraps. You might find it in a supermarket if it has a small car care section. Otherwise check your local automotive stores or a chemist or hardware. It is common stuff, should be easy to find.
BananeDC
B
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 15, Visits: 14
Can i find it in supermarkets ?

BananeDC
B
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 15, Visits: 14
ok thanks !

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As far as I can tell, white gas is pure petrol.  Petrol is not recommended for use on acrylic based plastics as it may dull the surface.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
BananeDC
B
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 15, Visits: 14
Thanks Warren. Is it ok with white gas ?

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
IPA is Iso-propyl alcohol.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
BananeDC
B
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 15, Visits: 14
Ok for the handle, thank you. Will send you an email.
Sorry, could you tell me what's IPA (I don't know the name in french)
I use white gas to clean silicone stains,  i have just checked on wikipedia, it says it does not attack plastics. Would you recommend it too ?

Edited 8 Years Ago by BananeDC
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The cost for the handle is £7.80 ex VAT. plus delivery to where ever you are in the world.

IPA is fine on the acrylic lid.  Avoid thinners as they can dissolve the plastic.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search