I am infusing ly556  resin and hy951 hardener with glass fibres to produce laminates of size 300mmx 150mm with 2 mm thickness. problem is as soon i open the resin line for infusion, resin accumulates around the line ad leaks out between bagging tape and vacuum bag. please help to resolve this problem
Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
This is very strange, as the pressure inside the bag during infusion should be lower than the atmospheric pressure. So the resin should not have any reason to flow out. Instead air should leak in. So I guess there are some problems with your setup

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
suman - 7 Years Ago
oekmont - 7 Years Ago
oekmont - 7 Years Ago
Warren (Staff) - 7 Years Ago
suman - 7 Years Ago
oekmont - 7 Years Ago
suman - 7 Years Ago
suman - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search