Kevin-Lee
Kevin-Lee
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 44,
Visits: 2.4K
Hi Joe,
Fantastic helmet!!! Way cooler than your average bit of kit...
Reply
Like
4
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Hi,
Thx guys for your nice comments.
@prairiecustoms: the band was cut to width, then I removed the outer 3k carbon tow (lengthwise, both sides of course). It's then tacked in place with masking tape wraped to become double side in the area of the mold where is the welding lens opening recess (dunno if it makes sense). I do not have tack spray so thats the only way I found to "secure" it relative to the mold. The ends of the band are secured to the mold flanges the same way.
For the rest, i just prayed the Composite God for the band not to move while laying the fabric layers. Seems I was lucky (but hey I prayed much).
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
5
Matthieu Libeert
Matthieu Libeert
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
nice work, looks great! did you use any varnish, topcoat on top? i'm finnishing my helmet these days
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
4
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Hey Matthieu, nice to hear about you! The helmet has its "out of the mold" bare epoxy finish. Cant wait to see your goalie in this showroom thread
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
4
FLD
FLD
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
Made some side scoops for my car. These are wet lay with a 200g outer layer for the nice pattern followed by 2 layers of 600g.
I also made some dash plates to replace the the manky silver ones which looked rather dated.
Reply
Like
5
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Quite cool
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
5
Matthieu Libeert
Matthieu Libeert
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Hi guys, so I finished my projects a few days ago, that I've started 6 months ago
It's a fieldhockey Keeper/goalie helmet made out of Carbon and Kevlar.
I've made 4 tutorials and will share them here, explaining the whole process of the making of.
Look at them if you'r interested...
Mouldmaking
Making backpart vacuumbagging
Making big part with VARTM technique
Finnishing part (fixing the problems I had with the Infusion)
shot with my new GoPro camera
Subscribe to my youtubechannel if you want direct updates on my projects
I can use any support!
Thanks to the help of the Easycomposites guys and all of you for all the inspiration and information found on this forum
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Tags
Carbon
Epoxy
Infusion
Kevlar
Vacuumbag
Reply
Like
6
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Hi Matthieu. I'm glad you finally made it! Looks quite nice, but should I ask for some front side pictures?
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
5
Matthieu Libeert
Matthieu Libeert
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Here are the additional pictures
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
4
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Haha, looks killer !
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
19
Prev
1
5
6
7
8
9
20
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search