Hi,
I did a mould using PU600 Density Polyurethane Model Board but end up having a mechanical lock when I tried to separate the mould from the board.
Apparently accetone can disolve  the polyurethane but  I was wandering if you guys have any advice?
cheers.

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Acetone won't touch polyurethane, only polystyrene. The only option is to grind either the tooling board or the mould away until you can break one of them off. This is generally pretty hard to do without damaging both surfaces, but it is otherwise start again from scratch.
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
We always recommend ensuring you have a small draught angle to the near vertical edges.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search